PORON 4701-50 materials are firm with excellent compression set resistance, providing shock and impact management.
This durable material can maintain its integrity and effectiveness, even when exposed to long periods of fluctuating temperatures.
When the focus is on gasket design, PORON 4701-50 foams are a top choice.
| PORON® 4701-50 Firm – Supported – Data Sheet | ||
|---|---|---|
| PROPERTY | TEST METHOD | VALUE |
| PHYSICAL | ||
| Density, kg /m3 (lb. / ft3) Tolerance, % | ASTM D 3574-95, Test A | 480 (30) ± 10 |
| Thickness, mm (inches) Tolerance, mm (inches) | 0.30 (0.012) 0.08 (± 0.003) |
|
| Standard Color (Code) | Black (04) | |
| Compression Force Deflection Range kPa (psi) Typical kPa (psi) | 0.51 cm/in (0.2” / min) Strain Rate Force Measured @ 25% Deflection | 103-310 (15-45) 221 (32) |
| Hardness, Durometer, Shore "O" | ASTM D 2240-97 | 55 |
| Compression Set, % max. | ASTM D 3574-95 Test D @ 23C (73F) ASTM D 3574-95 Test D @ 70C (158F) ASTM D 3574-95 Test J/Test D autoclaved 5 hrs @ 121C (250F) | 5 10 - |
| Dimensional Stability, % max. change | 22 hrs @ 80C (176F) in a forced-air oven | - |
| Tensile Strength, Min. kPa (psi) | ASTM D 3574-75 Test E | - |
| Tensile Elongation, % min. | ASTM D 3574-75 Test E | - |
| Tear Strength, Min. kN/m (pli), Typical kN/m (pli) | ASTM D 264-91 Die C | - |
| ELECTRICAL AND THERMAL | ||
| Dielectric Constant, K’ (“DK”) | ASTM D 150 measurements at 22C (72F) relative humidity 50% for 24 hrs. | 1.63 |
| Dielectric Strength, volts/mil | ASTM D 149-97a | 50 |
| Dissipation Factor, tan D (“DF”) | ASTM D 150-98 | 0.05 |
| Volume Resistivity, ohm-cm | ASTM D 257-99 | 2 x 1012 |
| Surface Resistivity, ohm/sq. | ASTM D 257-99 | 7 x 1012 |
| Thermal Conductivity, W/m-C (BTU-in./hr/ft2-F) | ASTM C 518-98 | 0.090 (0.63) |
| Coefficient of Thermal Expansion | 2.3 - 3.1 x 10-4 in/in/C (1.3-1.7 x 10-4 in/in/F | |
| TEMPERATURE RESISTANCE | ||
| Recommended Constant Use, max. | SAE J-2236 | 90°C (194°F) |
| Recommended Intermittent Use, max. | 121°C (250°F) | |
| Embrittlement | ASTM D 746-98 | -40°F (-40°C) |
| Cold Flexibility | MIL-P-12420D 1991 @ -40C (-40F) | Pass |
| PORON® 4701-50 Firm – Supported, Continued | ||
| PROPERTY | TEST METHOD | VALUE |
| FLAMMABILITY AND OUTGASSING | ||
| Flammability | UL 94HBF (File E20305) (Pass ) MVSS 302 (Pass ) CSA Comp HBF (File 188149) (Pass ) | - - - |
| Fogging | SAE J-1756 3 hrs @ 100C (212F) | Pass |
| Outgassing, Total Mass Loss (TML) % | ASTM E 595-93 24 hrs @ 125C (257F) @ <7x103 Pa | 0.9 |
| Outgassing, Collected Volatile Condensable Materials (CVCM) % | 0.06 | |
| Outgassing, Water Vapor Regain (WVR) % | 0.43 | |
| ENVIRONMENTAL | ||
| Gasketing and Sealing | UL JMST2 (Consisting of UL50 and UL508) CAN/CSA – C22.2 No. 94-M91 | File MH15464 - |
| Moisture Absorption, High Humidity Exposure, % weight gain, typical | AMS 3568-95 | 2 |
| Water Absorption, Immersion Testing, % weight gain, typical | ASTM D 570-95 | 5 |
| UV Resistance | ASTM G 53-96 | Good |
| Ozone Resistance | GM 4486P-95 | Pass |
| Corrosion Resistance | AMS 3568-91 | Pass |
| Mildew/Bacteria Resistance | ASTM G 21 | Good |
| Staining | ASTM D 925 | No Stain |
| Skin Contact Irritation | Primary Skin Irritation Test (FHSA) | Pass |
| PROPERTY | TEST METHOD | VALUE |
| Coefficient of Friction A/B, (Kinetic) | ASTM D 1894 | 0.4 |
| Density, kg /m3 (lb. / ft3) | ASTM D 1505 | 1.395 (87.1) |
| Modules, MD, kPa (psi) | ASTM D 882 | 3.5 x 106 (500,000) |
| Shrinkage, MD, %, (TD) | 39 min. at 150C (302 F) | 1.2 (0.0) |
| Tensile Strength, MD, kPa (psi) | ASTM D 882 | 2.1 x 105 (30,000) |
| Ultimate Elongation | ASTM D 882 | 150 |
| Yield Strength (F5), kPa (psi) | ASTM D 882 | 1.0 x 105 (15,000) |
| Brand | Item | Size |
|---|---|---|
| Rogers PORON | 4701-50-30012-04 | 1372mm*182.88m*0.3mm |
| Rogers PORON | 4701-50-30017-04 | 1372mm*144.68m*0.43mm |
| Rogers PORON | 4701-50-30020-04 | 1372mm*144.68m*0.5mm |
| Rogers PORON | 4701-50-30031-04 | 1372mm*45.72m*0.79mm |
| Rogers PORON | 4701-50-30045-04 | 1372mm*45.72m*1.14mm |
| Rogers PORON | 4701-50-20062-04 | 1372mm*91.44m*1.57mm |
| Rogers PORON | 4701-50-20093-04 | 1372mm*68.58m*2.36mm |
| Rogers PORON | 4701-50-20125-04 | 1372mm*50.29m*3.18mm |
| Rogers PORON | 4701-50-15188-04 | 1372mm*60.48m*4.78mm |
| Rogers PORON | 4701-50-15250-04 | 1372mm*24.38m*6.35mm |
| Rogers PORON | 4701-50-15375-04 | 1372mm*18.29m*9.53mm |
| Rogers PORON | 4701-50-15500-04 | 1372mm*12.19m*12.7mm |
Rogers offers a portfolio of thin, soft LCD Gasket solutions to seal and protect displays in TVs, monitors, tablets, and laptops.
Liquid Crystal Displays (LCDs) in display systems including large-screen televisions, computer monitors, laptops mobile phones, and other portable devices require protection and long-term performance of these important and delicate LCDs.
Display LCDs require cushioning, sealing, spacers, and grips to seal out dust and particulate matter, manage damaging impact energy to sensitive components, and keep the glass in place.